› Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation
Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation
Research article (Journal of Alloys and Compounds, 2023) · cited 52× · AI/ML
Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation
Summary
Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation is a scholarly article[1].
Key Facts
Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation. Retrieved May 24, 2026, from https://4ort.xyz/entity/microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur
MLA“Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur.
BibTeX@misc{4ortxyz_microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation}}, year = {2026}, url = {https://4ort.xyz/entity/microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Microstructure, texture and mechanical properties of Inconel GH4169 superalloy fabricated by wire arc additive manufacturing with arc oscillation — https://4ort.xyz/entity/microstructure-texture-and-mechanical-properties-of-inconel-gh4169-superalloy-fabricated-by-wire-arc-additive-manufactur (retrieved 2026-05-24)