Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy

Research article (Engineering Failure Analysis, 2018) · cited 68× · AI/ML
Press Enter · cited answer in seconds

Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy

Summary

Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy is a scholarly article[1].

Key Facts

  • Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy's instance of is recorded as scholarly article[2].

📑 Cite this page

Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.

APA 4ort.xyz Knowledge Graph. (2026). Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy. Retrieved May 24, 2026, from https://4ort.xyz/entity/effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy
MLA “Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy.
BibTeX @misc{4ortxyz_effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy}}, year = {2026}, url = {https://4ort.xyz/entity/effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy}, note = {Accessed: 2026-05-24}}
LLM prompt According to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Effects of grain size and texture on stress corrosion cracking of friction stir processed AZ80 magnesium alloy — https://4ort.xyz/entity/effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy (retrieved 2026-05-24)

Canonical URL: https://4ort.xyz/entity/effects-of-grain-size-and-texture-on-stress-corrosion-cracking-of-friction-stir-processed-az80-magnesium-alloy · Last refreshed: