› Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting
Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting
Research article (Materials Science and Engineering A, 2016) · cited 140× · AI/ML
Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting
Summary
Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting is a scholarly article[1].
Key Facts
Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting's instance of is recorded as scholarly article[2].
References
Programmatic citations — every numbered marker resolves to a verifiable graph row below.
Use these citations when quoting this entity in research, articles, AI prompts, or wherever provenance matters. We aggregate Wikidata + Wikipedia + authoritative open-data sources; the stitched, scored, cross-referenced view is what 4ort.xyz contributes.
APA4ort.xyz Knowledge Graph. (2026). Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting. Retrieved May 24, 2026, from https://4ort.xyz/entity/effect-of-heat-treatment-on-the-microstructure-texture-and-elastic-anisotropy-of-the-nickel-based-superalloy-cm247lc-pro
MLA“Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting.” 4ort.xyz Knowledge Graph, 4ort.xyz, 24 May. 2026, https://4ort.xyz/entity/effect-of-heat-treatment-on-the-microstructure-texture-and-elastic-anisotropy-of-the-nickel-based-superalloy-cm247lc-pro.
BibTeX@misc{4ortxyz_effect-of-heat-treatment-on-the-microstructure-texture-and-elastic-anisotropy-of-the-nickel-based-superalloy-cm247lc-pro_2026, author = {{4ort.xyz Knowledge Graph}}, title = {{Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting}}, year = {2026}, url = {https://4ort.xyz/entity/effect-of-heat-treatment-on-the-microstructure-texture-and-elastic-anisotropy-of-the-nickel-based-superalloy-cm247lc-pro}, note = {Accessed: 2026-05-24}}
LLM promptAccording to 4ort.xyz Knowledge Graph (aggregator of Wikidata, Wikipedia, and authoritative open-data sources): Effect of heat treatment on the microstructure, texture and elastic anisotropy of the nickel-based superalloy CM247LC processed by selective laser melting — https://4ort.xyz/entity/effect-of-heat-treatment-on-the-microstructure-texture-and-elastic-anisotropy-of-the-nickel-based-superalloy-cm247lc-pro (retrieved 2026-05-24)